Tungaloy Rev Up Turning Efficiency in Heat-Resistant Superalloys With New Ceramic Insert Grades

Tungaloy Rev Up Turning Efficiency in Heat-Resistant Superalloys With New Ceramic Insert Grades

Tungaloy Revs Up Turning Efficiency in Heat-Resistant Superalloys With New Ceramic Insert Grades

Tungaloy has unveiled two new ceramic insert grades: TS200 and TS300 that are developed for performing high-speed, high-efficiency turning operations of heat-resistant superalloys. The company has also introduced dedicated turning toolholders with a T-style insert clamp that are designed to securely hold the ceramic inserts to withstand demanding operations.

TS200 and TS300 are both SiAlON ceramic grades that are designed to perform high-speed turning operations of HRSAs common in aerospace, power generation and oil and gas industries. The TS200 is suitable for finishing processes; while the TS300 is ideal for removing oxide layer and other roughing operations.

The dedicated turning toolholders feature a unique T-style insert clamp with a carbide plate attached. This plate holds the ceramic insert securely in place in the seat to provide process security during demanding operations.

For other exclusive articles, visit www.equipment-news.com.

 

Check these articles out:

5G Integration In IIoT Systems Accelerates Industry 4.0 In The Wake Of Pandemic

Mouldmakers Turn To Process Automation In Race To Recover

TaeguTec: ChaseMold RTMX And RTHX Five-cutting Edge Insert Lines

Seco 335.18 And 335.19 Cutters Enable Smooth, Problem-Free Disc Milling

Tungaloy Enables Efficient Heavy-Duty Roughing of Difficult Materials

Coronavirus Hits Automotive And Aerospace Supply Chains

Wider Range for Heavy-duty Cutting Needs

 

WANT MORE INSIDER NEWS? SUBSCRIBE TO OUR DIGITAL MAGAZINE NOW!

FOLLOW US ON: LinkedIn, Facebook, Twitter

 

 

 

LVD Showcases New Products In Virtual Technology Events
TRUMPF And STMicroelectronics Partners For UWB Positioning Technology
Back To Top